baolidakj 等级:五级士官 累计积分:113 可用积分:113 |
楼主 发表于:2007-07-11 20:14:35 公司简介
石家庄开发区宝利达科技开发有限公司是一家集科、工、贸于一体的高新技术企业,主要从事化工、生物、制药、机电等高科技产品的研究、开发、应用。本公司科技实力雄厚,中、高级技术人员和中、高级管理人员占公司员工的80%,并与十余所著名大学建立了合作关系。公司引进、消化国外先进技术生产的绿康牌(LUKANG®)无机凝胶——硅酸镁锂(Hectorite),各项指标可与美国天然的硅酸镁锂和英国Laponite(B)人造硅酸镁锂相媲美,填补了国内空白,可取代进口产品,节约国家外汇。本公司的全体员工,本着“以质量求生存,以诚信求发展”的宗旨,“团结、奋进、开拓、进取”,用自己的勤劳和智慧,共同创造美好的明天。
Company Introduction
Shijiazhuang Development Zones Baolida Science & Technology Development Limited Company (hereafter referred to as “SDZB”) is a high technological company, which engaged in scientific research, manufacture and trade. The scope of its business mainly covers research, development and application of high technological products, such as chemicals, biological, pharmacy, and electromechanicals.
SDZB has an abundance of human resources of various kinds, medium, high-ranking technical people and administrator makes up 80% of the total company’s employee, and has established cooperative relation with more than 10 well-known universities.
SDZB introduce new techniques; manufacture Lithium magnesium silicate hydrate inorganic gel, or Hectorite (trade mark LUKANG®). The performance of LUKANG® Hectorite is approximate to America natural and lithium magnesium silicate hydrate and British Laponite (B) artificial one.
The staff of our company, in line with \" survive on high quality, aim on seek development with sincerity \", \" united, advance courageously, open up, keep forging ahead \", use one\'s own industry and intelligence, create beautiful tomorrow together.
产品说明Our Product
绿康凝胶学名:硅酸镁锂(Lithium magnesium silicate hydrate, or Hectorite) 是吸收国外高新技术,采用纳米工艺:溶胶——凝胶法,经人工合成的矿物质无机凝胶,为六方晶质结构,外观为白色粉末,无毒、无味,具有纳米特性。
LUKANG® gel (trade mark LUKANG®): lithium magnesium silicate hydrate or Hectorite ,SDZB introduce new techniques, synthesized it by sol-gel. It is supplied in the form of a white free-flowing fine powder, hexagonal lattice structure, innoxiously, tasteless, with nanometer property.
绿康凝胶具有独特的成胶性、触变性和吸附性,常作为增稠剂、悬浮剂、粘合剂、触变剂和分散剂使用,广泛用于化妆品、牙膏、洗涤用品、食品、医药、农药、生物、电子、涂料等日化、建材行业和工农业产品中,可降低生产成本,提高相关产品质量和品位,增加企业竞争力。绿康凝胶的技术参数达到了美国天然硅酸镁锂和英国Laponite(B)人造硅酸镁锂的指标。性能优于硅酸铝镁和市面上的类似产品。
LUKANG® gel is unique to colloid, thixotropy, and adsorbability , can be used as thickener, suspension agent and binder material, thixotropy agent, dispersing agent frequently, these unique properties are used to advantage in many applications: cosmetics , toothpaste , detergents, food, medicine, pesticide, biology, electron and coating .It can reduce production cost , raise related product quality and grade , increase enterprise competition ability.
The performance of LUKANG® Hectorite is approximate to America natural and Lithium magnesium silicate hydrate and British Laponite (B) artificial one, better than aluminum magnesium silicate hydrate and similar product.
绿康凝胶——即“绿康牌”硅酸镁锂的各项指标达到了欧洲化妆品标准(Dir.76/768/EEC)的要求,具体的M.S.D.S可与我们直接联系。
Data of LUKANG® gel has reached the requirement of European cosmetics standard (Dir.76/768/EEC); specific M.S.D.S can directly connect with us.
性能展示
Performance
绿康凝胶其性能特点如下:
LUKANG® gel’s performance characteristic is as follows:
1、性能稳定,抗降解:
1. Performance stabilization, unbreakable
绿康凝胶是非金属复合纳米材料,无机矿物质,不被细菌、加热和机械剪切破坏分解。在pH值为3-12范围的溶液中能够正常使用。
LUKANG® gel is nonmetal compound nanometer material, inorganic mineral substance, cannot be broken by bacteria, heat and mechanical shear. It can be used normally at pH value 3~12.
2、常温水合,节能、方便:
2. Hydration at room temperature, energy-saving, convenience
绿康凝胶能够在常温下与去离子水水合,膨胀成为悬浮的胶体,当浓度为1.5-2.5%时,形成透明或半透明的触变性凝胶。省去了加热工序,节能、方便。
LUKANG® gel can hydrate with demonized water to suspension colloid at room temperature, the suspension colloid turns into transparent or translucent thixotropic colloid at 1.5~2.5% solids content in water. Unheating, energy-saving and convenience.
3、胶体粘度高,用量小,成本低:
3.High viscosity colloid, a few dosages, low cost
绿康凝胶2.5%水悬浮液的粘度高达1500-3200mpa.s,而硅酸铝镁5%水悬浮液的粘度通常小于600mpa.s。因而,绿康凝胶固含量低、粘度高。使用绿康凝胶添加量小、成本低。
The viscosity of LUKANG® gel is 1500~ 3200mpa.s and the value of water suspension liquid of 5% of aluminum magnesium silicate hydrate is usually lower than 600mpa.s. So LUKANG® gel is low solids content, high viscosity, a few dosages and low cost.
4、配伍性好:
4.Excellent compatibility
绿康凝胶与大多数阴离子型表面活性剂及非离子型表面活性剂相溶性好,而和大多数阳离子型表面活性剂不相溶。绿康凝胶的水分散液,能够和可以以水相混溶的溶剂混合,如:20%的乙醇、50%的甘油等。绿康凝胶水分散液还可以与油类混合,形成油包水或水包油,但依赖于绿康凝胶的浓度和与油的比例。
LUKANG® gel shows excellent compatibility with most of anionic surfactant and nonionic surfactant, but incompatibility to most of cationic surfactant. The water dispersing solution of LUKANG® gel is compatible with water-miscible solvent, such as 20% ethanol, 50% glycerin water solution, and so on. The water dispersing solution of LUKANG® gel can mix with oil, thus water-in-oil or oil-in-water emulsion formed, that depend on the content of LUKANG® gel and oil.
5、改良有机增稠剂:
5. Modifying organic thickener
绿康凝胶与有机增稠剂一起使用时能发挥协调效应,获得最佳性能。绿康凝胶有助于协调粘度和屈服值,而有机增稠剂是在电解质、表面活性剂和其它水溶性物质存在的情况下改善绿康凝胶的稳定性,配合后的粘度和稳定性要比采用单一凝胶而得到的粘度和稳定性更好、更经济。绿康凝胶与羧甲基纤维素(CMC)混合性能曲线为:
LUKANG® gel may be used in combination with other organic thickeners where synergistic interactions can produce greatly improved efficiency and performance. LUKANG® gel is helpful for coordinative viscosity and yield value, and organic thickener can improve the stability of LUKANG® gel with the existence of electrolyte, surfactant and other water-soluble material, the stability and viscosity after coordination are better than before, and cost saving.
The performance curve of LUKANG® gel and carboxymethyl cellulose after mixed
6、增加稠度,改善粘度和肤感:
6. Increase thickness, improvement viscosity and skin sensation
绿康凝胶增稠效果显著,常用于膏霜、乳液类产品中作增稠剂,控制触变性和改善粘度,使稠密的膏霜流畅地涂抹。如:化妆品、牙膏、洗发膏、护肤、护发用品等。绿康凝胶还可改善化妆品的肤感,增加雅致感,降低或消除有机凝胶和聚合物的粘腻、胶质感或挂丝等。
Due to its notable thickening ability, LUKANG® gel can be thickener in cosmetic cream and emulsion frequently, to control thixotropy and improvement viscosity, make dense cosmetic cream smoothly on the skin. These include cosmetic, toothpaste, shampoo, skin and hair care agent. LUKANG® gel can improve skin sensation and elegance of cosmetic, reduce or eliminate the mucosity sensation of organic gel and polymer.
7、稳定悬浮液:
7. Stabilize suspension liquid
适当浓度的绿康凝胶在水性体系中可粘合、悬浮粉状物料(如:颜料、药物、滑石粉等),稳定悬浮液,防止已悬浮物质的沉淀积合、硬化,使悬浮液质地均匀,色泽艳丽,使用方便,喷雾更加容易,且不受外力、时间影响。
LUKANG® gel of proper density in water based system can adhesion and suspension powder materiel (such as pigment, medicine and talcum powder etc.), stabilize suspension liquid, prevent suspended material sediment and harden, make suspension liquid even, bright-colored, convenience, easy spraying, and unaffected by outside force and time.
8、做粘合剂和崩解剂:
8. Adhesive and disintegrant
绿康凝胶可做粘合剂和崩解剂,用于制造片状物、细园条物和经过压缩的饼状物块,能够保证粘结物块的质地均匀和期望的硬度、颜色,常用于制药等行业。绿康凝胶也起崩解剂的作用,在药剂和工业中将大块物崩解的更小,特别适用于大块物中主要组分占混合物的主要重量和容积的情况。
LUKANG® gel can be made adhesive, manufacture products with the shape of platelet, bar and cake, to guarantee the caking property pieces have expected quality, hardness and color; it is used in pharmacy frequently.
LUKANG® gel can be made disintegrant, disintegrate bulk material in medicament and industry, especially that primary constituent in bulk material is Major weight and volume in mixture.
9、良好的吸附作用:
9.Good adsorption
绿康凝胶具有良好的吸附作用,可吸附皮肤表面、口腔或身体中的有害细菌,强身健体。如用于面膜等护肤用品。
LUKANG® gel has good adsorption, it can adsorb harmful bacteria on skin surface, in oral cavity or body, keep you health. It can be used in face film and other skin care agent.
10、润肤、增白:
10.Moisten and whitened skin
绿康凝胶在化妆品中与甘油混合后能保水滋润皮肤,使皮肤变得细腻、光滑,增加皮肤的弹性,使皮肤增白。
When mixed with glycerol in cosmetic, LUKANG® gel can moisten skin, Make skin fine, smooth, increase the elasticity of skin, and whitened.
11、优化性能、降低成本:
11.Optimization performance and cost saving
绿康凝胶在牙膏中与CMC混合使用时能形成稳定的膏体、增进牙膏的触变性和分散性并改善出条结构,降低卡拉胶和CMC的用量;用于洗发香波,可减少助剂和油脂用量,减轻对皮肤的刺激,并降低成本。
When mixed with CMC in toothpaste, stabilized paste formed, LUKANG® gel can improve its thixotropy, dispersity and make the paste readily extruded from tube, low the consumption of carrageenan and CMC. Used in shampoo can reduce the consumption of assistant and oil, alleviate stimulability to skin, and reduce cost.
12、 其它:
12.Others
绿康凝胶中所含的微量元素——锂,用于化妆品可使皮肤变嫩变白;用于洗发香波具有护发和防止、治疗脱发的作用;用于牙膏可健龈洁齿。
The trace element Li that contained in LUKANG® gel, used in cosmetics can make skin tendered and white, used in shampoo can protect hair, prevent and treat alopecia, used in toothpaste can health gum and clean tooth.
13、安全性:
13.Safety
绿康凝胶是参照国内外类似产品标准,精选优级无机原料合成而成,达到了相关卫生标准。
LUKANG® gel refers to domestic and international similar product standard, select super grade inorganic raw material and have reached related sanitary standard.
绿康凝胶的主要性能指标
指标名称 指标
外观 白色、粉状、无味 白色、粉状、无味
理化指标 粘度(mpa.s)
(旋转式粘度计60转/分测定) 1500—3200
(2.5%水悬浮液)
pH值(2.5%水悬浮液) 10-11
炽灼失重% ≤17
干燥失重% ≤8
生化指标 细菌总数(个/g) ≤1000
大肠杆菌 无
重金属(Pb计)% ≤0.0015
砷(As) ≤0.0003
The main performance of LUKANG® gel
appearance white powder, tasteless
physicochemical parameter viscosity (mpa.s)
(rotational viscometer 60 r/m) 1500~3200
(2.5% water suspension colloid)
pH (2.5% water suspension colloid) 10~11
Ignition loss , wt% ≤17
Moisture content , wt% ≤8
Biochemical
parameter Total bacterial count(/g) ≤1000
Coli bacillus 0.0000
Pb,% ≤0.0015
As,% ≤0.0003
Hg,% ≤0.0001
联系我们
石家庄开发区宝利达科技开发有限公司
地址:石家庄市开发区友谊南大街349号
电话:0311-83018377 13131180287 13032636676
传真:0311-83018377邮编:050091
邮箱:public@baolidakj.cn
CONTACT US
Shijiazhuang Development Zones Baolida Science & Technology Development Limited Company
Address: 349 South Friendship Street, Development Zones, Shijiazhuang, P. R. China
Tel/ Fax: 0086-311-83018377
China Postcode: 050091
E-mail: chen@baolidakj.cn,
public@baolidakj.cn,
wang@baolidakj.cn,回复 1楼 |