金属铟丝 Indium wire Purity: 99.993%. Test result (For your reference): Cd: 5ppm; As:5ppm; Pb:8ppm; Sn:7ppm; Tl:5ppm; Fe:6ppm; Al:5ppm; Cu:5ppm; Zn:5ppm In:99.993% Diameter: 1mm/1.5mm/2mm. Packing: 1m/10m/20m per coil. 10coils per carton or as required. 联系人 倪成辉 倪成辉 13813001392 贸易通huanhuan53770 Qq 67443723 msn:huan5845201314@eyou.com E-mail:huan5845201314@126.com