nichenghui 等级:三级士官 累计积分:44 可用积分:44 |
楼主 发表于:2006-04-20 08:34:00 金属铟丝
Indium wire
Purity: 99.993%.
Test result (For your reference):
Cd: 5ppm;
As:5ppm;
Pb:8ppm;
Sn:7ppm;
Tl:5ppm;
Fe:6ppm;
Al:5ppm;
Cu:5ppm;
Zn:5ppm
In:99.993%
Diameter: 1mm/1.5mm/2mm.
Packing: 1m/10m/20m per coil. 10coils per carton or as required.
联系人 倪成辉
倪成辉 13813001392
贸易通huanhuan53770
Qq 67443723
msn:huan5845201314@eyou.com
E-mail:huan5845201314@126.com回复 1楼 |